Please use this identifier to cite or link to this item: http://hdl.handle.net/11375/27477
Title: Developing continuous submicron-scale conductive interpenetrating hydrogel network in polyethylene matrices through controlled crazing and polymerization
Authors: Kornberg, Anton
Thompson, Michael
Zhu, Shiping
Department: Chemical Engineering
Publication Date: 12-Mar-2020
Publisher: Industrial and Engineering Chemistry Research
Abstract: An approach is described for the synthesis of controlled submicron interpenetrating networks with distinct functional features in commodity polymers, based on a mechanism of crazing and polymerization. In this work, ion conductivity was introduced into polyethylene with only minor losses in its mechanical properties, using a highly branched acrylic hydrogel. Control over the porous network developed in the matrix was gained by the addition of a crystallizing nucleating agent, which was used to increase the number and reduce the size of crystallites. Variation of experimental conditions, such as the degree of elongation and applied reaction pressure, produced different morphologies and conductivity for the co-continuous alloy. The samples were deformed in a liquid medium that possessed an affinity for the matrix material, and acted both as a surface-active agent for the crazing, and as a reactant for the conductive phase. Without pressure, deforming by 100% strain yielded a conductivity of 5.67×10⁻⁷ S/cm for the polymer specimen. Simultaneously increasing system pressure while constantly straining a specimen enabled further enhancements in conductivity. As a particular example, elongation of 100% and applied pressure up to 2.76 MPa ensured conductivity nearly equal to that of the pure hydrogel at 4.43×10⁻⁴ S/cm.
URI: http://hdl.handle.net/11375/27477
Identifier: https://doi.org/10.1021/acs.iecr.9b07010
Appears in Collections:Faculty Publications

Files in This Item:
File Description SizeFormat 
Revised Manuscript_I&ECR_Feb_29.pdf
Open Access
1.88 MBAdobe PDFView/Open
Show full item record Statistics


Items in MacSphere are protected by copyright, with all rights reserved, unless otherwise indicated.

Sherman Centre for Digital Scholarship     McMaster University Libraries
©2022 McMaster University, 1280 Main Street West, Hamilton, Ontario L8S 4L8 | 905-525-9140 | Contact Us | Terms of Use & Privacy Policy | Feedback

Report Accessibility Issue