Skip navigation
  • Home
  • Browse
    • Communities
      & Collections
    • Browse Items by:
    • Publication Date
    • Author
    • Title
    • Subject
    • Department
  • Sign on to:
    • My MacSphere
    • Receive email
      updates
    • Edit Profile


McMaster University Home Page
  1. MacSphere
  2. Open Access Dissertations and Theses Community
  3. Digitized Open Access Dissertations and Theses
Please use this identifier to cite or link to this item: http://hdl.handle.net/11375/25739
Full metadata record
DC FieldValueLanguage
dc.contributor.advisorWilkinson, D.S.-
dc.contributor.advisorWeatherly, G.C.-
dc.contributor.authorJin, Qiang-
dc.date.accessioned2020-08-28T13:52:17Z-
dc.date.available2020-08-28T13:52:17Z-
dc.date.issued1995-08-
dc.identifier.urihttp://hdl.handle.net/11375/25739-
dc.description.abstractThe compressive creep behaviour of a high purity silicon nitride ceramic with and without the addition of Ba was studied at 1400°C. Two distinct creep stages were observed during high temperature deformation of these materials. The stress exponents for creep of the two materials indicate that they have different creep mechanisms during the second stage of creep. Cavitation during creep was determined by measuring the density change before and after creep using a water­-displacement method. The Ba doped material exhibited an obvious density decrease, indicating cavitation during creep, whereas the undoped material exhibited no cavitation. This is consistent with TEM observations. The microstructure of the materials, especially the amorphous grain-boundary phase was investigated for both as-sintered and crept specimans by means of transmission electron microscopy (TEM). Statistical analysis of a number of grain-­boundary films indicates that the film thickness is confined to a narrow range (standard deviation less than 0.15 nm) in the as-sintered materials. The average film thickness depends on film chemistry, increasing from 1.0 nm to 1.4 nm when Ba is added. The standard deviation of the film thickness of a given material after creep, however, is considerably larger than before (0.30 nm ~ 0.59 nm). This suggests that the grain-boundary glass phase is redistributed during creep. Viscous flow of the glass phase is proposed as die mechanism responsible for the first stage of creep. The data are compared with a model for viscous creep, yielding good correlation.en_US
dc.language.isoenen_US
dc.subjecthigh temperatureen_US
dc.subjectcreep deformationen_US
dc.subjectsilicon nitride ceramicsen_US
dc.titleHigh Temperature Creep Deformation of Silicon Nitride Ceramicsen_US
dc.typeThesisen_US
dc.contributor.departmentMaterials Science and Engineeringen_US
dc.description.degreetypeThesisen_US
dc.description.degreeMaster of Engineering (ME)en_US
Appears in Collections:Digitized Open Access Dissertations and Theses

Files in This Item:
File Description SizeFormat 
Jin_Qiang_1995Aug_Masters.pdf
Open Access
3.65 MBAdobe PDFView/Open
Show simple item record Statistics


Items in MacSphere are protected by copyright, with all rights reserved, unless otherwise indicated.

Sherman Centre for Digital Scholarship     McMaster University Libraries
©2022 McMaster University, 1280 Main Street West, Hamilton, Ontario L8S 4L8 | 905-525-9140 | Contact Us | Terms of Use & Privacy Policy | Feedback

Report Accessibility Issue